Having understood the different requirements of market, we have developed Chequered Plywood Sheet of the good quality. It is very useful for developing other products out of it. Also, prices are economical and it broad and strong.
STONIC Chequered plywood is a combination of high quality Gurjan veneer and imported birch veneer panels treated with high viscous phenol formaldehyde resin, with a steel wire mesh and phenolic overlay with a GSM of 40 to 250 g/m2. STONIC Chequered plywood is a slip resistant. Our Chequered Plywood if a highly demanding product by transport applications.
The base plywood of our chequered plywood is normally made of cross-bonded 1.4 mm thick birch veneers / Gurjan veneers. We use the large size core and panels for minimum core gap and smooth top surface impression. This also increase the bonding strength among the veneers and gives ultimate strength to product. A durable phenolic film is hot-pressed onto the panel surface. Standard colour is dark brown / Black 220 g/m2. The reverse side is a smooth phenolic brwon / black film.
STONIC Chequered Plywood surface is always with smooth diamond patterned. The surface is hard and withstands abrasion and rolling wear, is moisture resistant and can tolerate commonly used chemicals as well as diluted acids and alkalis. The surface is easy to clean with water or steam.
Applications of Chequered Plywood AS109 :
Major Advantages of Chequered Plywood AS109:
Available Dimensions of Chequered Plywood AS109:
Properties of Chequered Plywood AS109 :
PROPERTIES | RESULTS | VALUE |
Density | IS: 1708 (Part-2) - 1986 | 1.1 |
Moisture content and volatile content | IS: 1708 (Part-1) - 1986 | 9% |
Water absorption in 24 hrs. | AS: 109.63 : Feb. 2003 | 3% |
Cross breaking strength | | |
Along the grain | IS: 1998 ( ) : 1962 | 1300 kg/cm2 |
Tensile strength | | |
Along the grain | IS: 1734 (Part-9) - 1983 | 900 kg/cm2 |
Compressive strength | AS: 109: 63 Feb:2002 | 900 kg/cm2 |
Izode impact test | IS: 1708 (Part-I) - 1986 | Pass the test |
Parallel to laminate | | 65 kg/cm2 |
Perpendicular to laminate | | 40 kg/cm2 |
Swelling in boiling water after 8 hrs. | AS: 109: 63 Feb. 2002 | 10% |